ASTM A872 UNS J93550 Stainless Steel Pipe
+
  • ASTM A872 UNS J93550 Stainless Steel Pipe

ASTM A872 UNS J93550 Stainless Steel Pipe

ASTM A872 UNS J93550 Steel Pipe covers centrifugally cast ferritic/austenitic steel pipe intended for general corrosive service.Which are susceptible to embrittlement if used for prolonged periods at elevated temperatures.

Key Word:

Steel Pipe

Products Detial

Standard:ASTM A872/A872M

Standard Specification for Centrifugally Cast Ferritic/Austenitic Stainless Steel Pipe for Corrosive Environments

ASTM A872 UNS J93550 Steel Pipe covers centrifugally cast ferritic/austenitic steel pipe intended for general corrosive service.

ASTM A872 UNS J93550 Steel Pipe are susceptible to embrittlement if used for prolonged periods at elevated temperatures.

ASTM A872 UNS J93550 Stainless Steel Pipe Quick Details

Company Name: beite steel pipe

Country/Region: China

Product Name:ASTM A872 UNS J93550 Stainless Steel Pipe

Manufacture:centrifugal casting process.

Outside Diameter:34mm——219mm

Wall thickness:5.4mm——21mm

Length:6000mm、12000m or specified length as require

Port of Shipment:Tianjin,China

Payment:L/C or T/T

Delivery: 7-15 days after payment

Package: Bundles (hexagonal),Wooden Boxes,Crates (steel/wooden)

Materials and Manufacture

Manufacture:

The pipes are made by the centrifugal casting process.

Machining

The pipes are machined on the inner surface and may be supplied either machined or unmachined in the outer surface. 

Heat Treatment

All pipes shall be furnished in the heat-treated condition as shown in Table 1.

TABLE 1 Heat Treatment Requirements

 

Grade Condition 
Temperature,
°F [°C]
Quenching
UNS J93550 1920–2100 [1050–1150] Water quench or rapid
cooling by other means

Chemical Composition of ASTM A872 UNS J93550 Stainless Steel Pipe

Element Grade  
UNS J93550
C 0.030
Mn 2.0
P 0.040
S 0.030
Si 2.0
Ni 5.00–8.00
Cr 23.0–26.0
Mo 2.00–4.00
N 0.08–0.25
Cu 1.00
Co 0.50–1.50

Mechanical Properties of ASTM A872 UNS J93550 Stainless Steel Pipe

 

Requirement Grade
UNS J93550
Tensile strength, min, ksi [MPa] 90 [620]
Yield strength, min, ksi [MPa] 65 [450]
Elongation in 2 in. or 50 mm, min,% 20
Hardness, max:  
Brinell 297
Rockwell C 31.5

Quality

The surface of the casting shall be examined visually and shall be free of cracks and hot tears. 

Permissible Variations in Dimensions

Thickness—The wall thickness shall not vary over that specified by more than 1 ⁄ 8 in. [3 mm]. There shall be no variation under the specified wall thickness.

Packaging 

Bundles (hexagonal),

Wooden Boxes,

Crates (steel/wooden)

The tubing be packaged or bundled in such a manner as to prevent damage in ordinary handling and transportation and identified by a tag with the name of the manufacturer, purchase order number, specification number and grade, and size.

Factory Photo

our factory
our factory
our factory
our factory

Online Inquiry

Please fill in the form to get more information as soon as possible

Action

Enter product details, such as color, size, material, etc., and other specific requirements to obtain accurate quotations.

Send inquiry now

*Attention: Please fill in the information accurately and keep communication open. We will contact you as soon as possible

Submit